← HistoryWhich outcome resulted when early Chinese cast iron cannons encountered manufacturing flaws?
A)Catastrophic barrel rupture occurred✓
B)Propellant burned more slowly
C)Cast iron became more brittle
D)Projectile range was unaffected
💡 Explanation
Catastrophic barrel rupture was more common due to uneven cooling rates which induced residual stresses via thermal expansion; because tensile strength was exceeded, cannons failed explosively rather than deforming plastically or functioning normally under normal conditions.
🏆 Up to £1,000 monthly prize pool
Ready for the live challenge? Join the next global round now.
*Terms apply. Skill-based competition.
Related Questions
Browse History →- Which environmental factor most significantly accelerated the deterioration via efflorescence of Mesopotamian Ziggurats constructed primarily from mud brick?
- Which systematic error arises when an astrolabe's alidade sighting vanes are misaligned during celestial altitude measurement?
- In Aztec chinampa agriculture, which primary outcome resulted from disrupted soil particle aggregation?
- Which mechanical failure was prevalent in early Mesopotamian bronze agricultural plowshares during abrasive soil tilling?
- Which risk arises when weathering erodes lime mortar affecting pietra dura inlay?
- Which consequence results when ships experienced hogging forces?