← TechnologyWhich risk increases when accelerated hydration significantly elevates early-age temperature in concrete columns?
A)Delayed ettringite formation✓
B)Chloride-induced reinforcement corrosion
C)Increased compressive strength
D)Alkali-silica reaction propagation
💡 Explanation
When accelerated hydration elevates early-age temperature, the delayed ettringite formation (DEF) risk increases greatly because high temperatures destabilize the initial ettringite structure, creating conditions for delayed formation. Therefore, DEF is the primary risk rather than corrosion, increased strength, or alkali-silica reaction which depend on different environmental factors.
🏆 Up to £1,000 monthly prize pool
Ready for the live challenge? Join the next global round now.
*Terms apply. Skill-based competition.
Related Questions
Browse Technology →- Which performance reduction occurs when an HVAC evaporator coil ices over completely?
- Which outcome is caused when a refrigeration system uses a zeotropic refrigerant blend during evaporator coil flooding?
- Which outcome occurs when an undersized accumulator responds to fluctuating demand?
- Which risk increases when hydraulic actuator demand exceeds the local pump's flow capacity?
- Which outcome occurs from exceeding a commercial airliner's critical mach number during descent?
- Which consequence results when ultrasonic fuel injection deposits form in gasoline direct injection (GDI) engine injectors?