← ScienceWhich outcome can result from continued Galvanic corrosion?
A)Formation of new ionic compounds✓
B)Passivation layer thickening
C)Electrode redox potential reversal
D)Increased grain boundary diffusion
💡 Explanation
Continued galvanic corrosion erodes the anode through ion transfer via oxidation, leading to formation of new ionic compounds (rust), because electron transfer drives the corrosion, therefore compound form rather than passivation; this occurs elsewhere. Other conditions produce the other reactions.
🏆 Up to £1,000 monthly prize pool
Ready for the live challenge? Join the next global round now.
*Terms apply. Skill-based competition.
Related Questions
Browse Science →- Which effect occurs near black holes because of extreme gravity?
- Which energy output occurs if the strong force overcomes electrostatic repulsion during deuterium-tritium fusion?
- Which outcome occurs when high concentrations of product inhibit an enzyme-catalyzed reaction in a closed system?
- Which consequence results when U-235 undergoes neutron-induced fission?
- Which phenomenon causes blurring in quantum mechanical simulations of molecular dynamics when using coarse-grained wave functions?
- Which constraint on reaction rate arises when enriched uranium-235 causes control rod failure in a nuclear reactor?