← ScienceWhich risk increases when a turbine blade's gamma prime (γ') precipitates coarsen in the nickel-based superalloy lattice?
A)Reduced high-temperature creep resistance✓
B)Increased susceptibility to oxidation
C)Elevated thermal conductivity threshold
D)Enhanced fatigue delamination tolerance
💡 Explanation
Reduced creep resistance occurs because γ' precipitate coarsening decreases dislocation pinning, driving creep via grain boundary sliding rather than plastic deformation of precipitates. Therefore, creep resistance lowers; rather than increased oxidation because precipitate coarsening primarily affects mechanical properties.
🏆 Up to £1,000 monthly prize pool
Ready for the live challenge? Join the next global round now.
*Terms apply. Skill-based competition.
Related Questions
Browse Science →- Which risk increases when a MOSFET's gate oxide layer decreases?
- Which outcome occurs when an adiabatic flash drum receives a high-enthalpy liquid stream with insufficient residence time?
- Which risk increases when a chiller using R-134a reaches low suction pressure?
- Which outcome occurs when measuring spin on one entangled electron destroys coherence?
- Which process limits electronic conductivity in solid-state ionic conductors at low temperatures?
- Which risk increases when tokamak plasma composition shifts with high-Z isotopes?